Cause analysis and solution of plastic shell dent

Release time:2022-02-28

During the injection molding process, the dents of the plastic shell are shrinkage dents generated after the plastic is cooled and hardened, which mainly appear in the thick wall of the plastic shell, ribs, shell, nut insert back, etc.

3.jpg


1、 Equipment:

(1) Insufficient feeding

The screw or plunger is seriously worn, and the molten material leaks during the injection and pressure maintaining process, which reduces the mold filling pressure and the amount of molten material, resulting in insufficient molten material.


(2) Nozzle hole too large or too small

If it is too small, it is easy to block the sprue; if it is too large, the injection force is small, and it is difficult to fill the mold.


2、 Mold:

(1) The gate is too small or the runner is too narrow or shallow, the runner efficiency is low, the resistance is large, and the molten material is cooled too early.

The gate cannot be too large, otherwise the shear rate will be lost, the material viscosity is high, and the plastic shell will not be full. The gate should be opened on the thick wall of the plastic shell. By setting up a cold charging well with sufficient capacity in the flow channel, the cold charging can be excluded from entering the mold cavity, so that the mold filling can continue.

The gate length of point gate and needle gate must be controlled below 1mm, otherwise the plastic will solidify rapidly in the gate, affecting the pressure transmission; If necessary, increase the number of point gates or gate positions to meet the actual needs; When the flow passage is long and thick, exhaust grooves should be set at the edge of the flow passage to reduce the blocking effect of air on the flow of materials.


(2) Multi gate mold should adjust the filling speed of each gate, and it is best to set up gates symmetrically.


(3) The key parts of the mold should be effectively set with cooling channels to ensure that the cooling of the mold has a good effect on removing or reducing shrinkage cavities.


(4) The whole mold should be free of burrs, have reliable mold closing tightness, and can withstand the filling of high-pressure, high-speed, low viscosity molten materials.


3、 Technical aspects:

(1) Increase the injection pressure, maintain the pressure and prolong the injection time.

For plastic with high fluidity, high pressure will cause flash and collapse, so the material temperature should be appropriately reduced, and the temperature of the front of the barrel and the nozzle should be reduced, so that the volume change of molten material entering the cavity is reduced, and it is easy to cold solidify; For high viscosity plastics, the barrel temperature should be increased to make it easier to fill the mold. When the gate area shrinks, the pressure holding time should be extended.


(2) Increasing the injection speed can easily fill the parts and remove most of the shrinkage.


(3) The thin-walled plastic shell should increase the mold temperature to ensure the smooth flow of materials; The thick wall plastic shell should reduce the mold temperature to accelerate the curing and shaping of the skin.


(4) The cooling residence time of the plastic shell in the mold is prolonged, the production cycle is kept uniform, the back pressure is increased, and a certain buffer pad is reserved at the front end of the screw, which is conducive to reducing the shrinkage phenomenon.


(5) The low precision plastic shell should be taken out of the mold as soon as possible and cooled slowly in air or hot water, so that the shrinkage depression can become smooth without affecting the use.


4、 Raw materials:

The raw material is too soft and easy to flow. The effective way is to add nucleating agent to the plastic to accelerate crystallization.


5、 Plastic shell design:

The design of plastic shell should make the wall thickness uniform and try to avoid the change of wall thickness. For plastics with large shrinkage such as polypropylene, when the thickness changes by more than 50%, it is best to replace the thickened part with ribs.

Copyright: Shenzhen Zhongyuan Plastic Co., Ltd. | mold processing customized manufacturer. If you want to know the processing price of the factory, how much is it, and which is good, please contact us Yue ICP Bei No. 17060480
主站蜘蛛池模板: 日夜啪啪| 日韩免费精品一级毛片 | 亚洲国产影院 | 青草青青产国视频在线 | 天堂√在线中文资源网 | 天天干视频网站 | 亚洲高清国产一线久久 | 五月婷婷丁香在线 | 特黄特黄aaaa级毛片免费看 | 天堂亚洲网 | 日本红怡院亚洲红怡院最新 | 色亚洲成人 | 天天干 夜夜操 | 欧美怡春院一区二区三区 | 四虎成人在线 | 青娱乐国产精品视频 | 污污的视频在线免费观看 | 中文字幕波多野结衣免费视频 | 色综合视频在线 | 亚洲成人欧美 | 亚洲刺激视频 | 午夜性福 | 亚洲最新网址 | 日本道v高清免费 | 天天做天天躁天天躁 | 特级淫片欧美高清视频蜜桃 | 天天爱天天做天天干 | 全国男人的天堂网 | 欧美在线视频不卡 | 婷婷网五月天天综合天天爱 | 亚欧乱色精品免费观看 | 日本高清高色 | 西欧毛片| 天堂网在线新版www 天堂网在线网站成人午夜网站 | 欧洲一区在线观看 | 无码精品日韩中文字幕 | 亚欧人成精品免费观看 | 日日噜噜噜夜夜爽爽狠狠 | 一级做a毛片免费视频 | 日日夜夜精品免费视频 | 午夜影院私人 |